Flame-retardant PP Modified Materials | Flame-retardant PE Modified Materials | Flame-retardant ABS Modified Materials | Antistatic Masterbatches | PPA Lubricating and Anti-blocking Masterbatches | Silicone Lubricating Masterbatches | PPO Modified Materials | PP Anti-aging Modified Materials | PE Anti-aging Modified Materials

全国咨询热线:400-167-5355 +86-571-82138550


Address: No. 489, Getai 6th Road, Xiaoshan Economic Development Zone, Hangzhou, Zhejiang, China. 
Tel: +86-571 - 82138550
Fax: +86-571 - 82859550

Website: www.hafukeji.com



您当前的位置:网站首页  >  新闻资讯  >  常见问题

为什么添加了PE吹膜阻燃母粒的薄膜,接缝线痕迹明显 故障分析及排除方法:

(1) 机头或机头连接器温度太高。应适当降低。但温度不能太低,否则,仍会产生接缝线。

(2) 芯棒尖端部位有焦料粘附。应修改芯棒尖端部位的形状,使其圆滑过渡。

(3) 机头机构设计不合理。应修改机头设计。

地址:No. 489, Hongtai 6th Road, Xiaoshan Economic Development Zone, Hangzhou,Zhejiang, China.
服务热线:400-167-5355 +86-571-82138550   传真:+86-571-82859550

Copyright © 2024 Jinwei Nano New Material (Hangzhou) Co.,Ltd All rights reserved. 备案号:Zhejiang ICP No. 16005835-1
技术支持:杭州哈博信息技术有限公司

免费咨询