Flame-retardant PP Modified Materials | Flame-retardant PE Modified Materials | Flame-retardant ABS Modified Materials | Antistatic Masterbatches | PPA Lubricating and Anti-blocking Masterbatches | Silicone Lubricating Masterbatches | PPO Modified Materials | PP Anti-aging Modified Materials | PE Anti-aging Modified Materials
注塑成型时主流道粘模的原因及排除方法:
(1)冷却时间太短,主流道尚未凝固。
(2)主流道斜度不够,应增加其脱模斜度。
(3)主流道衬套与射嘴的配合尺寸不当造成漏流。
(4)主流道粗糙,主流道无冷却井。
(5)射嘴温度过低,应提高温度。